| 0.2% Proof Stress | 550 N/mm2 | 
| Tensile Strength | 750 N/mm2 | 
| Elongation, 5.65√S0 | 25% | 
| Reduction of area | 45% | 
| Hardness (Brinell) | 270 max. | 
| Impact Strength (Room Temp) | 80J | 
| Impact Strength (-46oC) | 60J av (45J min) | 
	
| Density (Kg/m3) | 7810 | 
| Magnetic Permeability (20°C) | 33 | 
| Young’s Modulus (kN/mm2) | 199 | 
| Specific Electrical Resistance, 20°C (µΩ.m) | 0.8 | 
| Mean coefficient of thermal expansion, 20-300°C (m/m/oC) | 11.1 x 10-6 | 
| Specific Heat, 20°C (J/kg.K) | 475 | 
| Thermal conductivity, 20°C (W/m.K) | 14.2 | 
| Fracture Toughness, kQ (MPa/m2) | 98 |